dc.description.abstractMetakaolin, fly ash, and mostly granulated blast furnace slag (GBFS) are traditionally used in the production of geopolymer. This study, adding to the knowledge base on geopolymer concretes as an alternative to cement mixtures, explored an experimental approach that investigates the use of ceramic dust (CD) and rice husk ash (RHA) with high SiO content instead of GBFS in the production of geopolymers. For this purpose, instead of GBFS, RHA at proportions of 0, 5%, 10%, and 15% and CD at proportions of 0, 10%, 20%, and 30% were used in the production of geopolymer concrete. In addition, groups were determined with a Taguchi L16 matrix with NaOH (an important material in geopolymer production) at 12, 14, 16, and 18 molality. Varying combinations of flow diameter, density, porosity, and water absorption rate were used, and their performance under high temperatures in terms of compressive strength was evaluated. The use of RHA in geopolymer concretes produced using CD and RHA had a negative effect on the flow and water absorption rates. However, the use of CD had a positive effect, and geopolymer concretes with high density and porosity were obtained. In addition, it was determined that strengths > 70 MPa could only be obtained if 5-20% CD were used at 14-16 molality. The resistance of geopolymer concretes to high temperatures is lower than normal concretes. However, when comparing RHA and CD, it was determined that the use of CD would be more effective on geopolymer materials, and special measures should be taken at temperatures > 450 °C.
dc.identifier.doi10.1007/s11356-021-16869-w
dc.identifier.eissn1614-7499
dc.identifier.endpage15895
dc.identifier.issn0944-1344
dc.identifier.pubmed34633616
dc.identifier.scopus2-s2.0-85116923819
dc.identifier.startpage15876
dc.identifier.urihttps://hdl.handle.net/20.500.12597/11890
dc.identifier.volume29
dc.identifier.wosWOS:000706053800020
dc.relation.ispartofEnvironmental Science and Pollution Research
dc.relation.ispartofENVIRONMENTAL SCIENCE AND POLLUTION RESEARCH
dc.rightsfalse
dc.subjectCompressive strength
dc.titleTaguchi optimization of geopolymer concrete produced with rice husk ash and ceramic dust.
dc.titleTaguchi optimization of geopolymer concrete produced with rice husk ash and ceramic dust
dc.typeJournal Article
dspace.entity.typePublication
oaire.citation.issue11
oaire.citation.volume29
relation.isPubmedOfPublication7f24724b-a363-489e-9cc2-01f441d336a6
relation.isPubmedOfPublication.latestForDiscovery7f24724b-a363-489e-9cc2-01f441d336a6
relation.isScopusOfPublicationa62e31a0-bf94-4220-8b91-021e02c16e0c
relation.isScopusOfPublication.latestForDiscoverya62e31a0-bf94-4220-8b91-021e02c16e0c
relation.isWosOfPublicationfc69e079-1a1d-4820-91c1-1de010e631f6
relation.isWosOfPublication.latestForDiscoveryfc69e079-1a1d-4820-91c1-1de010e631f6

Files

Collections