dc.description.abstractThe letter reports that frequency response of heterojunction structure based on a spin-coated graphenePVP thin film on silicon with gold Schottky contacts and the electronic properties obtained by using capacitance (C) and conductance (G/omega) versus voltage characteristics in the frequency range from 5 to 5 MHz. Furthermore, the electronic magnitudeswere calculated. The accumulation capacitance observed at 3 V changes from 920 to 1094 pF. Here, empirically, the C and G/omega values increased with a decreasing frequency, while increasing in depletion and accumulation regions with increasing voltages. However, particularly, the R-s-V-f curves have peaks in low frequency values in the accumulationand depletion regions, these peaks decreased at high frequencies. Besides, an interface trap state density of 5.6-6.58x10(12) cm(-2).eV(-1) with a relaxation time constant of 157-31.5 mu s was deduced. Additionally, the frequencyand dc bias voltage-dependent dielectric characteristics show a huge dispersion, at room temperature. Experimentally, the high dielectric constant (epsilon(max)') is 111 which is very higher than themaximum value of the conventionalmaterials (SiO2 (3.8), SnO2 (7.5), and so on) and appropriatedopedmaterials to PVP. The results indicate that the graphene-PVP thin film with the high epsilon(max)' max value has a potential in metalorganic-semiconductors device technologies instead of a conventional device.
dc.description.urihttps://doi.org/10.1109/ted.2021.3129722
dc.description.urihttps://dx.doi.org/10.1109/ted.2021.3129722
dc.description.urihttps://avesis.gazi.edu.tr/publication/details/98cc9856-5595-4071-b701-c5db5a6c6d32/oai
dc.identifier.doi10.1109/ted.2021.3129722
dc.identifier.eissn1557-9646
dc.identifier.endpage310
dc.identifier.issn0018-9383
dc.identifier.openairedoi_dedup___::03ebcfb00a2b9c6fae896cf5bc04d8c1
dc.identifier.orcid0000-0002-2765-4165
dc.identifier.scopus2-s2.0-85120550246
dc.identifier.startpage304
dc.identifier.urihttps://hdl.handle.net/20.500.12597/39337
dc.identifier.volume69
dc.identifier.wos000727917900001
dc.publisherInstitute of Electrical and Electronics Engineers (IEEE)
dc.relation.ispartofIEEE Transactions on Electron Devices
dc.rightsCLOSED
dc.titleHigh Dielectric Performance of Heterojunction Structures Based on Spin-Coated Graphene-PVP Thin Film on Silicon With Gold Contacts for Organic Electronics
dc.typeArticle
dspace.entity.typePublication
local.api.response{"authors":[{"fullName":"Osman Cicek","name":"Osman","surname":"Cicek","rank":1,"pid":{"id":{"scheme":"orcid","value":"0000-0002-2765-4165"},"provenance":null}},{"fullName":"Gizem Koca","name":"Gizem","surname":"Koca","rank":2,"pid":null},{"fullName":"Semsettin Altindal","name":"Semsettin","surname":"Altindal","rank":3,"pid":null}],"openAccessColor":null,"publiclyFunded":false,"type":"publication","language":{"code":"und","label":"Undetermined"},"countries":null,"subjects":[{"subject":{"scheme":"FOS","value":"0103 physical sciences"},"provenance":null},{"subject":{"scheme":"FOS","value":"01 natural sciences"},"provenance":null}],"mainTitle":"High Dielectric Performance of Heterojunction Structures Based on Spin-Coated Graphene-PVP Thin Film on Silicon With Gold Contacts for Organic Electronics","subTitle":null,"descriptions":["The letter reports that frequency response of heterojunction structure based on a spin-coated graphenePVP thin film on silicon with gold Schottky contacts and the electronic properties obtained by using capacitance (C) and conductance (G/omega) versus voltage characteristics in the frequency range from 5 to 5 MHz. Furthermore, the electronic magnitudeswere calculated. The accumulation capacitance observed at 3 V changes from 920 to 1094 pF. Here, empirically, the C and G/omega values increased with a decreasing frequency, while increasing in depletion and accumulation regions with increasing voltages. However, particularly, the R-s-V-f curves have peaks in low frequency values in the accumulationand depletion regions, these peaks decreased at high frequencies. Besides, an interface trap state density of 5.6-6.58x10(12) cm(-2).eV(-1) with a relaxation time constant of 157-31.5 mu s was deduced. Additionally, the frequencyand dc bias voltage-dependent dielectric characteristics show a huge dispersion, at room temperature. Experimentally, the high dielectric constant (epsilon(max)') is 111 which is very higher than themaximum value of the conventionalmaterials (SiO2 (3.8), SnO2 (7.5), and so on) and appropriatedopedmaterials to PVP. The results indicate that the graphene-PVP thin film with the high epsilon(max)' max value has a potential in metalorganic-semiconductors device technologies instead of a conventional device."],"publicationDate":"2022-01-01","publisher":"Institute of Electrical and Electronics Engineers (IEEE)","embargoEndDate":null,"sources":["Crossref"],"formats":null,"contributors":null,"coverages":null,"bestAccessRight":{"code":"c_14cb","label":"CLOSED","scheme":"http://vocabularies.coar-repositories.org/documentation/access_rights/"},"container":{"name":"IEEE Transactions on Electron Devices","issnPrinted":"0018-9383","issnOnline":"1557-9646","issnLinking":null,"ep":"310","iss":null,"sp":"304","vol":"69","edition":null,"conferencePlace":null,"conferenceDate":null},"documentationUrls":null,"codeRepositoryUrl":null,"programmingLanguage":null,"contactPeople":null,"contactGroups":null,"tools":null,"size":null,"version":null,"geoLocations":null,"id":"doi_dedup___::03ebcfb00a2b9c6fae896cf5bc04d8c1","originalIds":["10.1109/ted.2021.3129722","50|doiboost____|03ebcfb00a2b9c6fae896cf5bc04d8c1","3216954381","98cc9856-5595-4071-b701-c5db5a6c6d32","50|od_____10046::190e6c5f8b53758d138393ea5b037d02"],"pids":[{"scheme":"doi","value":"10.1109/ted.2021.3129722"}],"dateOfCollection":null,"lastUpdateTimeStamp":null,"indicators":{"citationImpact":{"citationCount":9,"influence":3.0010852e-9,"popularity":9.211255e-9,"impulse":9,"citationClass":"C5","influenceClass":"C5","impulseClass":"C4","popularityClass":"C4"}},"instances":[{"pids":[{"scheme":"doi","value":"10.1109/ted.2021.3129722"}],"license":"IEEE Copyright","type":"Article","urls":["https://doi.org/10.1109/ted.2021.3129722"],"publicationDate":"2022-01-01","refereed":"peerReviewed"},{"alternateIdentifiers":[{"scheme":"doi","value":"10.1109/ted.2021.3129722"},{"scheme":"mag_id","value":"3216954381"}],"type":"Article","urls":["https://dx.doi.org/10.1109/ted.2021.3129722"],"refereed":"nonPeerReviewed"},{"alternateIdentifiers":[{"scheme":"doi","value":"10.1109/ted.2021.3129722"}],"type":"Article","urls":["https://avesis.gazi.edu.tr/publication/details/98cc9856-5595-4071-b701-c5db5a6c6d32/oai"],"publicationDate":"2022-01-01","refereed":"nonPeerReviewed"}],"isGreen":false,"isInDiamondJournal":false}
local.import.sourceOpenAire
local.indexed.atWOS
local.indexed.atScopus

Dosyalar

Koleksiyonlar