Yayın:
Mechanical durability and microstructural properties of sustainable high strength mortars ıncorporated basalt fiber and copper slag: Taguchi optimization

dc.contributor.authorAbu Aeshah, Mohammed Naji Ahmed
dc.contributor.authorKaplan, Gökhan
dc.date.accessioned2026-01-04T17:01:33Z
dc.date.issued2022-07-01
dc.description.abstractThis study produced high strength and low CO2 emission mortars using copper slag (CS) as aggregate and Supplementary Cementitious Materials (SCMs). It aims to develop a more environmentally friendly product by using CS both as aggregate and SCMs simultaneously. In addition, it is reinforced with basalt fiber (BF) so that copper waste does not adversely affect its mechanical and durability properties. Taguchi L18 orthogonal test matrix was used in the experimental study. CS was used at 25 and 50% instead of natural aggregate, 7.5%, and 15% instead of cement. BF was added to the mixture in 6 and 12 mm lengths at 1, 2, and 3 ratios. 91-day compressive strengths of the mixtures vary between 41 and 77 MPa. As a result of the optimization, a mixture with a 91-day compressive strength of 81 MPa was obtained. Na2SO4-induced expansions decreased if 15% CS was used instead of cement. Since the water absorption of CS is lower than that of natural aggregate, excessive strength losses after freezing-thawing are prevented. When CS is used as aggregate, drying shrinkage values increase because it reduced the aggregate volume. Air voids smaller than 200 nm were observed in SEM images. It is appropriate to use 7.5% when CS instead of cement and up to 25% when used instead of aggregate. On the other hand, it is appropriate to use up to 2% of BF at a length of 6 mm. Mixtures with a compressive strength of 50 MPa and above can be produced by using CS.
dc.description.urihttps://doi.org/10.1016/j.conbuildmat.2022.127815
dc.description.urihttps://avesis.atauni.edu.tr/publication/details/bfa87db5-557a-4d6d-b2d8-9e924191fc6c/oai
dc.identifier.doi10.1016/j.conbuildmat.2022.127815
dc.identifier.issn0950-0618
dc.identifier.openairedoi_dedup___::69ce39da5a1599b14f7cef5c65563cfd
dc.identifier.orcid0000-0001-6067-7337
dc.identifier.scopus2-s2.0-85130377856
dc.identifier.startpage127815
dc.identifier.urihttps://hdl.handle.net/20.500.12597/39842
dc.identifier.volume339
dc.identifier.wos000804098100001
dc.language.isoeng
dc.publisherElsevier BV
dc.relation.ispartofConstruction and Building Materials
dc.rightsCLOSED
dc.titleMechanical durability and microstructural properties of sustainable high strength mortars ıncorporated basalt fiber and copper slag: Taguchi optimization
dc.typeArticle
dspace.entity.typePublication
local.api.response{"authors":[{"fullName":"Abu Aeshah, Mohammed Naji Ahmed","name":"Mohammed Naji Ahmed","surname":"Abu Aeshah","rank":1,"pid":null},{"fullName":"KAPLAN, Gökhan","name":"Gökhan","surname":"Kaplan","rank":2,"pid":{"id":{"scheme":"orcid","value":"0000-0001-6067-7337"},"provenance":null}}],"openAccessColor":null,"publiclyFunded":false,"type":"publication","language":{"code":"eng","label":"English"},"countries":null,"subjects":[{"subject":{"scheme":"FOS","value":"0211 other engineering and technologies"},"provenance":null},{"subject":{"scheme":"FOS","value":"02 engineering and technology"},"provenance":null}],"mainTitle":"Mechanical durability and microstructural properties of sustainable high strength mortars ıncorporated basalt fiber and copper slag: Taguchi optimization","subTitle":null,"descriptions":["This study produced high strength and low CO2 emission mortars using copper slag (CS) as aggregate and Supplementary Cementitious Materials (SCMs). It aims to develop a more environmentally friendly product by using CS both as aggregate and SCMs simultaneously. In addition, it is reinforced with basalt fiber (BF) so that copper waste does not adversely affect its mechanical and durability properties. Taguchi L18 orthogonal test matrix was used in the experimental study. CS was used at 25 and 50% instead of natural aggregate, 7.5%, and 15% instead of cement. BF was added to the mixture in 6 and 12 mm lengths at 1, 2, and 3 ratios. 91-day compressive strengths of the mixtures vary between 41 and 77 MPa. As a result of the optimization, a mixture with a 91-day compressive strength of 81 MPa was obtained. Na2SO4-induced expansions decreased if 15% CS was used instead of cement. Since the water absorption of CS is lower than that of natural aggregate, excessive strength losses after freezing-thawing are prevented. When CS is used as aggregate, drying shrinkage values increase because it reduced the aggregate volume. Air voids smaller than 200 nm were observed in SEM images. It is appropriate to use 7.5% when CS instead of cement and up to 25% when used instead of aggregate. On the other hand, it is appropriate to use up to 2% of BF at a length of 6 mm. Mixtures with a compressive strength of 50 MPa and above can be produced by using CS."],"publicationDate":"2022-07-01","publisher":"Elsevier BV","embargoEndDate":null,"sources":["Crossref"],"formats":null,"contributors":null,"coverages":null,"bestAccessRight":{"code":"c_14cb","label":"CLOSED","scheme":"http://vocabularies.coar-repositories.org/documentation/access_rights/"},"container":{"name":"Construction and Building Materials","issnPrinted":"0950-0618","issnOnline":null,"issnLinking":null,"ep":null,"iss":null,"sp":"127815","vol":"339","edition":null,"conferencePlace":null,"conferenceDate":null},"documentationUrls":null,"codeRepositoryUrl":null,"programmingLanguage":null,"contactPeople":null,"contactGroups":null,"tools":null,"size":null,"version":null,"geoLocations":null,"id":"doi_dedup___::69ce39da5a1599b14f7cef5c65563cfd","originalIds":["S095006182201488X","10.1016/j.conbuildmat.2022.127815","50|doiboost____|69ce39da5a1599b14f7cef5c65563cfd","bfa87db5-557a-4d6d-b2d8-9e924191fc6c","50|od______9933::1f9a87d66f41903e71127d66d88dd062"],"pids":[{"scheme":"doi","value":"10.1016/j.conbuildmat.2022.127815"}],"dateOfCollection":null,"lastUpdateTimeStamp":null,"indicators":{"citationImpact":{"citationCount":9,"influence":2.8890397e-9,"popularity":9.336188e-9,"impulse":9,"citationClass":"C5","influenceClass":"C5","impulseClass":"C4","popularityClass":"C4"}},"instances":[{"pids":[{"scheme":"doi","value":"10.1016/j.conbuildmat.2022.127815"}],"license":"Elsevier TDM","type":"Article","urls":["https://doi.org/10.1016/j.conbuildmat.2022.127815"],"publicationDate":"2022-07-01","refereed":"peerReviewed"},{"alternateIdentifiers":[{"scheme":"doi","value":"10.1016/j.conbuildmat.2022.127815"}],"type":"Article","urls":["https://avesis.atauni.edu.tr/publication/details/bfa87db5-557a-4d6d-b2d8-9e924191fc6c/oai"],"publicationDate":"2022-07-01","refereed":"nonPeerReviewed"}],"isGreen":false,"isInDiamondJournal":false}
local.import.sourceOpenAire
local.indexed.atWOS
local.indexed.atScopus

Dosyalar

Koleksiyonlar