Yayın: Effects of B Addition on the Microstructure and Microhardness of Melt-Spun Al-7075 Alloy
| dc.contributor.author | Kilicaslan, Muhammed Fatih | |
| dc.contributor.author | Elburni, Saad Ibrahim | |
| dc.contributor.author | Yilmaz, Yasin | |
| dc.contributor.author | Akkaş, Mehmet | |
| dc.date.accessioned | 2026-01-04T16:52:40Z | |
| dc.date.issued | 2022-06-01 | |
| dc.description.abstract | Abstract Main aim of this study is to examine change of microstructural and the mechanical properties of Al-7075 alloy depending on B content added with different proportions. Rapid solidification process used to produce the alloys was carried out with a single roll melt spinner via a wheel with a rotational speed of 25 m/s. For the microstructural characterization of the alloys, a scanning electron microscope and X-ray diffraction analyzes were used. According to obtained results, it can be said that B addition led to modification of dimensions and shapes of both α−Al and intermetallic phases occurred, it reduced average grain size from 0.45 μm to 0.34 μm in the microstructure. The B addition also led to dramatically increase in microhardness of the Al-7075 alloy. The microhardness of the alloy with 0.4 wt. % B is 0.19 GPa, this is clearly one times higher than that of the alloy without B addition. The microhardness of the alloy with 1 wt. % B is 0.21 GPa, this is also slightly higher than that of the alloy with 0.4 wt. % B. | |
| dc.description.uri | https://doi.org/10.2478/adms-2022-0004 | |
| dc.identifier.doi | 10.2478/adms-2022-0004 | |
| dc.identifier.eissn | 2083-4799 | |
| dc.identifier.endpage | 18 | |
| dc.identifier.openaire | doi_________::6d5a0bc951be6daa3c7efaf358474869 | |
| dc.identifier.startpage | 5 | |
| dc.identifier.uri | https://hdl.handle.net/20.500.12597/39741 | |
| dc.identifier.volume | 22 | |
| dc.identifier.wos | 000826622000001 | |
| dc.language.iso | eng | |
| dc.publisher | Walter de Gruyter GmbH | |
| dc.relation.ispartof | Advances in Materials Science | |
| dc.rights | OPEN | |
| dc.title | Effects of B Addition on the Microstructure and Microhardness of Melt-Spun Al-7075 Alloy | |
| dc.type | Article | |
| dspace.entity.type | Publication | |
| local.api.response | {"authors":[{"fullName":"Muhammed Fatih Kilicaslan","name":"Muhammed Fatih","surname":"Kilicaslan","rank":1,"pid":null},{"fullName":"Saad Ibrahim Elburni","name":"Saad Ibrahim","surname":"Elburni","rank":2,"pid":null},{"fullName":"Yasin Yilmaz","name":"Yasin","surname":"Yilmaz","rank":3,"pid":null},{"fullName":"Mehmet Akkaş","name":"Mehmet","surname":"Akkaş","rank":4,"pid":null}],"openAccessColor":"gold","publiclyFunded":false,"type":"publication","language":{"code":"eng","label":"English"},"countries":null,"subjects":[{"subject":{"scheme":"FOS","value":"0203 mechanical engineering"},"provenance":null},{"subject":{"scheme":"FOS","value":"0103 physical sciences"},"provenance":null},{"subject":{"scheme":"FOS","value":"02 engineering and technology"},"provenance":null},{"subject":{"scheme":"FOS","value":"01 natural sciences"},"provenance":null}],"mainTitle":"Effects of B Addition on the Microstructure and Microhardness of Melt-Spun Al-7075 Alloy","subTitle":null,"descriptions":["<jats:title>Abstract</jats:title> <jats:p>Main aim of this study is to examine change of microstructural and the mechanical properties of Al-7075 alloy depending on B content added with different proportions. Rapid solidification process used to produce the alloys was carried out with a single roll melt spinner via a wheel with a rotational speed of 25 m/s. For the microstructural characterization of the alloys, a scanning electron microscope and X-ray diffraction analyzes were used. According to obtained results, it can be said that B addition led to modification of dimensions and shapes of both α−Al and intermetallic phases occurred, it reduced average grain size from 0.45 μm to 0.34 μm in the microstructure. The B addition also led to dramatically increase in microhardness of the Al-7075 alloy. The microhardness of the alloy with 0.4 wt. % B is 0.19 GPa, this is clearly one times higher than that of the alloy without B addition. The microhardness of the alloy with 1 wt. % B is 0.21 GPa, this is also slightly higher than that of the alloy with 0.4 wt. % B.</jats:p>"],"publicationDate":"2022-06-01","publisher":"Walter de Gruyter GmbH","embargoEndDate":null,"sources":["Crossref"],"formats":null,"contributors":null,"coverages":null,"bestAccessRight":{"code":"c_abf2","label":"OPEN","scheme":"http://vocabularies.coar-repositories.org/documentation/access_rights/"},"container":{"name":"Advances in Materials Science","issnPrinted":null,"issnOnline":"2083-4799","issnLinking":null,"ep":"18","iss":null,"sp":"5","vol":"22","edition":null,"conferencePlace":null,"conferenceDate":null},"documentationUrls":null,"codeRepositoryUrl":null,"programmingLanguage":null,"contactPeople":null,"contactGroups":null,"tools":null,"size":null,"version":null,"geoLocations":null,"id":"doi_________::6d5a0bc951be6daa3c7efaf358474869","originalIds":["10.2478/adms-2022-0004","50|doiboost____|6d5a0bc951be6daa3c7efaf358474869"],"pids":[{"scheme":"doi","value":"10.2478/adms-2022-0004"}],"dateOfCollection":null,"lastUpdateTimeStamp":null,"indicators":{"citationImpact":{"citationCount":4,"influence":2.661426e-9,"popularity":4.9269926e-9,"impulse":4,"citationClass":"C5","influenceClass":"C5","impulseClass":"C5","popularityClass":"C4"}},"instances":[{"pids":[{"scheme":"doi","value":"10.2478/adms-2022-0004"}],"license":"CC BY NC ND","type":"Article","urls":["https://doi.org/10.2478/adms-2022-0004"],"publicationDate":"2022-06-01","refereed":"peerReviewed"}],"isGreen":false,"isInDiamondJournal":false} | |
| local.import.source | OpenAire | |
| local.indexed.at | WOS |